Kiln Firing Success!
The second firing of the Ramsey Dragon Kiln was a great success! We reached temperature in the back of the Kiln in 48 hours and then threw wood in the side ports and maintained temp in the front for another 12 hours. Making for a 60 hour firing!
This has been 7 years in the making...
Now the 300 pieces have to cool for a week until we can unload the Kiln.